• Cost reduction

• Reduce Chemicals Level

• Uniform quality

• Low processing cost: Rapid breakdown during mixing, low power consumption during mixing, mixing faster, short curing cycle

• Improve processing: Minimum shrinkage and swell, Increase extrusion and calendaring rates, Blister-free calendaring for heavy gauges, Quick dispersion in high solid mastics, Reduce processing temperature

• Reduce scrap: Non scorchy compound

GRADE
COLOR
REFINATION
RAW MATERIAL
CHEMICAL ANALYTICAL DATA:
ACETONE EXTRACT (%)
ASH (%)
CARBON BLACK (%)
MOISTURE: LESS THAN (%)
RUBBER HYDROCARBON (%)
( BY DIRRERENCE )
PHYSICAL PROPERTIES OF THE
VULCANIZED RECLAIM:
SPECIFIC GRAVITY (AT 25°C)
MOONEY VISCOSITY
( ML 1’ + 4' @ 100°C)
HARDNESS (SHORE A)
TENSILE STRENGTH -KG/CM2
                      "                 -PSI
                      "                 -MPA
ELONGATION (%)
TEST RECIPES:
RECLAIMED RUBBER
(100 RHC) 100.00 PHR
STEARIC ACID 2.00 PHR
ZINC OXIDE 5.00 PHR
MBT 0.50 PHR
DPG 0.20 PHR
SULPHUR 3.00 PHR
CURED AT 20’ AT 142°C (287° F)
IN THE HYDRAULIC PRESS



Reclaimed rubber is a type of rubber recycled from waste or worn-out manufactured rubber articles. Read more..

 


Black recycled nylon is mainly made of recycled nylon 6 from tire cord. It still has essential properties compared to virgin nylon. Read more..

Rubber powder is made from waste or worn-out rubber products, mainly unusable tires. Read more..

 

 
 